Pressure Treated Wood Question
Posted: Mon Sep 02, 2024 8:47 am
by HenryFan
Last month, I bought another utility trailer and it has a pressure treated wood deck. 2X6 pressure treated pine I believe.
I was so new when I bought it, you could smell the paint and the wood.
I want to apply some sort of wood preservative to the deck and I seek comments on how long I should wait for the wood to dry before I apply a treatment.
I am familiar with Thompson's Water Seal, does that seem to be good option?
Not related to firearms but comments are appreciated.
Thanks - HenryFan
Re: Pressure Treated Wood Question
Posted: Mon Sep 02, 2024 9:01 am
by JEBar
I use Thompson's on the wooden floors of our various trailers .... I usually apply the first coat when the wood reaches the point it readily soaks in the Thompson's .... where possible be sure to seal the ends and sides of the boards .... I've not found it worth the effort seal the bottom of the boards
Re: Pressure Treated Wood Question
Posted: Mon Sep 02, 2024 10:06 am
by Cowboy Gun Fan
The general rule I would go by for new pressure treated wood is to wait 6 months for it to dry out before applying anything to it.
I also like Thompson's Water Seal.
Re: Pressure Treated Wood Question
Posted: Mon Sep 02, 2024 10:55 am
by HenryFan
Thanks for the above comments.
Is any preparation(s) advisable before applying the product other than scrubbing the deck with something like dish detergent?
Re: Pressure Treated Wood Question
Posted: Mon Sep 02, 2024 11:05 am
by BigAl52
If you want to seal it with something that I think is way better than Thompsons use Penefin. Its more expensive but will outlast Thompsons by a long shot.
Re: Pressure Treated Wood Question
Posted: Mon Sep 02, 2024 11:15 am
by HenryFan
BigAl - Thanks
Re: Pressure Treated Wood Question
Posted: Mon Sep 02, 2024 11:59 am
by Cowboy Gun Fan
HenryFan wrote: ↑Mon Sep 02, 2024 10:55 am
Thanks for the above comments.
Is any preparation(s) advisable before applying the product other than scrubbing the deck with something like dish detergent?
If you are using an Oil Base product, you don't want to use anything water before using it. It needs to be very dry to properly absorb it.
Re: Pressure Treated Wood Question
Posted: Mon Sep 02, 2024 3:17 pm
by Mags
HenryFan wrote: ↑Mon Sep 02, 2024 8:47 am
Last month, I bought another utility trailer and it has a pressure treated wood deck. 2X6 pressure treated pine I believe.
...
There might be a stamp from the lumber mill on the wood that tells you the pressure treated grade. If it is "Ground Contact" or better, you don't need to add to it.
Otherwise Penofin as Al suggested is very good, specifically Penofin Ultra Premium Red Label. Thompson's won't hold up to wear and tear, heat or UV. It'll break down and start flaking. You'll end up wanting to redo the wood with something else and you'll find the residual Thompson that hasn't started flaking hard to remove.
Re: Pressure Treated Wood Question
Posted: Mon Sep 02, 2024 10:39 pm
by The Happy Kaboomer
I treated my trailer wood floor with diesel fuel and burnt motor oil........Has held very well out in the weather....No cracks or splits......And can be re-applied as often as you want.
Re: Pressure Treated Wood Question
Posted: Thu Sep 05, 2024 3:18 pm
by Redthies
JEBar wrote: ↑Mon Sep 02, 2024 9:01 am
I've not found it worth the effort seal the bottom of the boards
I don’t do a thing to pressure treated lumber and live in a far harsher climate than most of you guys. If you do decide to seal it, you want to seal both sides, both edges and both ends. Otherwise, you are just wasting money. If you leave one edge unsealed, the moisture will just come in from there and rot will commence as if you didn’t seal it at all.