Thanks to all ,PT7 wrote:Looks like you've done some good homework, and your casting is coming along nicely.
Good work...appreciate seeing/learning through your experiences.
One more thing. At least to my recall, first time I've seen your new avatar. Looks !
Have a good day.
PT7
BruniX wrote:the main difficulty is to keep the mold at the right temperature, neither too hot nor too cold.
Also, i have spent a lot of time , before to obtain very clean alloy, by fluxing lead, making ingots etc ....
new avatar for wrangler rank, now...
but no more gun at all , waiting more for 45-70 brass lever action....
(seems very hard to find, according to my reseller)
But i want a henry for first riffle, or no riffle at all
at this speed, i will have lot of ammo when it come at home